How to Reduce Plastic Injection Molding Defects
Most repeat defects are visible in the CAD or the unchecked tolerance block.
Before steel
Uniform walls, draft, and a gate plan. A DFM review is cheaper than a texture repair. Nominal wall choice, thick-to-thin transitions and rib ratios are covered in our wall thickness guidelines. Definitions, causes and floor-level fixes for sink, flash, short shots and related injection molding defects are in our molding defects guide; this page is about reducing them in design and at trial.
At trial
Change one family of settings at a time and record it. If the defect does not move, it is probably steel or geometry.